- The aluminum A201 alloy with the T7 heat treat has the lowest
density, but it cannot meet the tensile strength requirement specified in the design.
In addition, the aluminum
has the lowest values for modulus of elasticity and hardness and the corrosion resistance
is rated as fair
|