A Design Study in Austempered Ductile Iron - Smith Foundry Drive Wheel

No Bake Sand Molding

The no bake sand mold meets and exceeds the production requirements for dimensional tolerance, surface finish, and intricacy of detail on the drive wheel.

But there is a cost disadvantage in mold prep time, sand reclamation, and overall mold production cost, compared to green sand molding. 

No bake sand is not the best choice.
Go Back for Another Choice!
 