      1.  The molten steel (2850F)  is poured into the assembled sand mold and allowed to
      cool and solidify in the mold.
 2. 
      After
      cooling, the casting is removed and "shaken
      out" of the sand mold.
 3. 
      The risers are cut  off and the riser stubs and flash lines are ground
      smooth.
 4. 
      The
      casting is shot-blasted for surface appearance. 
         |