| 5.  The vacuum is
      released from the pattern carrier and the  vacuum-constrained mold is
      stripped off  the pattern. 
     | 6.  The two mold
      halves (cope and drag) are joined together to form the completed plastic
      lined mold cavity.  The vacuum is maintained in the flasks during
      molten metal pouring. 
     |