10%
    SiC Addition to Aluminum  | 
   
 
 
  
     | 
    
      The aluminum with
        10% SiC addition meets the minimum requirements for modulus and strength, compared to the
        unreinforced C 355-T6. 
       
      The fluidity of the
        aluminum with 10% SiC addition exceed the minimum fluidity requirements at the 775C
        pouring temperature. 
                  --  It is
        approximately 10% more fluid  
                      than
        the Al-20% SiC alloy. 
       
      But  the specific modulus (modulus
        divided by the density) for the 10% SiC addition is 11% lower than the
        specific modulus for the 20% SiC addition (127.7 x 10^6 vs 143.1 x 10^6 in) 
       
     
     | 
   
 
 
  
  |