sfsa_s.gif (4934 bytes)

amc.gif (6172 bytes) afs.gif (3195 bytes)
A Design Study in Steel - Crossbleed Valve for the F-5

Casting, Cutting, and Cleaning 

The valve body is cast in a four step process.

1.  The molten steel is poured into the ceramic mold and allowed to cool and solidify.

2.  After cooling, the  ceramic mold is removed (knock-out) from the casting. 

3.  The gates are cut off the casting and the stubs and flash lines are ground smooth.

4.  The casting is shot-blasted clean for surface appearance

Metal Being Poured by Hand into the Mold

 The Finished Casting Before Cutting


Back


Next

24

 
Copyright 2007 by the Steel Founders' Society of America.
All rights reserved.  Address comments to: 
blairr@sfsa.org
Last Modified:December, 2007 by STG

arrow_top.gif (1191 bytes)