1.
Preheat the steel mold and coat the mold interior with the refractory ceramic coating (applied as a
spray slurry).
2.
Melt the metal in the furnace.
3.
Rotate the mold, pour the metal, and spin the mold until the casting
solidifies.
4.
Remove the casting from the mold after solidification.
5.